MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

IIMAK METALLOGRAPH™ IINK-SSX Conductive Ink
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This electrically conductive screen ink has been developed for use in printed electronics, notably for membrane switches, flexible circuits, electroluminescent lighting and other applications requiring fine line features. This product features market-leading dry times and temperatures and has excellent flexibility and adhesion to a variety of substrates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.43 g/cc0.160 lb/in³
Solids Content 62 - 63 %62 - 63 %
Filler Content 53.25 - 53.75 %53.25 - 53.75 %Silver (Ag)
Particle Size 6.0 µm6.0 µm
Viscosity 49000 - 51000 cP49000 - 51000 cP
Thickness 1.00 - 10.0 microns0.0394 - 0.394 mil
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000052 - 0.000057 ohm-cm0.000052 - 0.000057 ohm-cm
Surface Resistivity per Square 0.015 - 0.045 ohm0.015 - 0.045 ohm
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.00 %0.00 %
 
Processing PropertiesMetricEnglishComments
Cure Time 2.00 - 7.00 min0.0333 - 0.117 hour
 
Descriptive Properties
Adhesion5
Binder SystemProprietary
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Solvent Systemglycol ethers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFLEXCM30 / 179432

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.