MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polycarbonate, Extruded
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.03 - 1.26 g/cc0.0372 - 0.0455 lb/in³Average value: 1.20 g/cc Grade Count:102
 1.02 - 1.02 g/cc
@Temperature 290 - 300 °C
0.0368 - 0.0368 lb/in³
@Temperature 554 - 572 °F
Average value: 1.02 g/cc Grade Count:4
Water Absorption 0.0200 - 0.350 %0.0200 - 0.350 %Average value: 0.162 % Grade Count:35
Moisture Absorption at Equilibrium 0.120 - 0.350 %0.120 - 0.350 %Average value: 0.151 % Grade Count:40
Water Absorption at Saturation 0.300 - 0.400 %0.300 - 0.400 %Average value: 0.319 % Grade Count:20
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/dayAverage value: 15.0 g/m²/day Grade Count:10
Oxygen Transmission 65.0 - 2760 cc-mm/m²-24hr-atm165 - 7010 cc-mil/100 in²-24hr-atmAverage value: 863 cc-mm/m²-24hr-atm Grade Count:9
Nitrogen Transmission 12.0 - 510 cc-mm/m²-24hr-atm30.5 - 1300 cc-mil/100 in²-24hr-atmAverage value: 159 cc-mm/m²-24hr-atm Grade Count:9
Carbon Dioxide Transmission 380 - 16900 cc-mm/m²-24hr-atm965 - 42900 cc-mil/100 in²-24hr-atmAverage value: 5230 cc-mm/m²-24hr-atm Grade Count:9
Viscosity  800000 - 800000 cP
@Temperature 320 - 320 °C
800000 - 800000 cP
@Temperature 608 - 608 °F
Average value: 800000 cP Grade Count:1
 800000 - 800000 cP
@Shear Rate 25.0 - 25.0 1/s
800000 - 800000 cP
@Shear Rate 25.0 - 25.0 1/s
Average value: 800000 cP Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cm0.00200 - 0.00900 in/inAverage value: 0.00638 cm/cm Grade Count:57
Linear Mold Shrinkage, Transverse 0.00500 - 0.00800 cm/cm0.00500 - 0.00800 in/inAverage value: 0.00705 cm/cm Grade Count:28
Melt Flow 1.00 - 25.0 g/10 min1.00 - 25.0 g/10 minAverage value: 8.79 g/10 min Grade Count:69
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 70.0 - 75.070.0 - 75.0Average value: 71.7 Grade Count:12
Hardness, Rockwell R 114 - 124114 - 124Average value: 119 Grade Count:14
Ball Indentation Hardness 95.0 - 120 MPa13800 - 17400 psiAverage value: 112 MPa Grade Count:13
Tensile Strength, Ultimate 28.0 - 75.0 MPa4060 - 10900 psiAverage value: 65.9 MPa Grade Count:68
Tensile Strength, Yield 39.0 - 120 MPa5660 - 17400 psiAverage value: 62.7 MPa Grade Count:74
Elongation at Break 6.10 - 138 %6.10 - 138 %Average value: 88.6 % Grade Count:82
Elongation at Yield 3.00 - 60.0 %3.00 - 60.0 %Average value: 9.05 % Grade Count:65
Modulus of Elasticity 1.58 - 3.24 GPa229 - 470 ksiAverage value: 2.31 GPa Grade Count:66
Flexural Yield Strength 36.0 - 103 MPa5220 - 15000 psiAverage value: 88.6 MPa Grade Count:59
Flexural Modulus 0.971 - 3.10 GPa141 - 450 ksiAverage value: 2.28 GPa Grade Count:86
Flexural Strain at Break 7.00 - 7.20 %7.00 - 7.20 %Average value: 7.10 % Grade Count:4
Flexural Strain at Yield 7.00 - 7.20 %7.00 - 7.20 %Average value: 7.10 % Grade Count:10
Compressive Yield Strength 18.0 - 86.2 MPa2610 - 12500 psiAverage value: 49.0 MPa Grade Count:3
Izod Impact, Notched 0.481 - 9.61 J/cm0.900 - 18.0 ft-lb/inAverage value: 6.75 J/cm Grade Count:30
 5.00 - 6.78 J/cm
@Temperature -51.1 - 0.000 °C
9.37 - 12.7 ft-lb/in
@Temperature -60.0 - 32.0 °F
Average value: 4.68 J/cm Grade Count:3
 2.72289 - 2.72289 J/cm
@Temperature -40.0 - -40.0 °C
5.10109 - 5.10109 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 4.68 J/cm Grade Count:1
 2.72289 - 2.72289 J/cm
@Thickness 3.17 - 3.17 mm
5.10109 - 5.10109 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 4.68 J/cm Grade Count:1
Izod Impact, Notched (ISO) 10.0 - 90.0 kJ/m²4.76 - 42.8 ft-lb/in²Average value: 64.7 kJ/m² Grade Count:45
 10.0 - 16.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.76 - 7.61 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 13.6 kJ/m² Grade Count:27
 12.0 - 20.0 kJ/m²
@Temperature -30.0 - -30.0 °C
5.71 - 9.52 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 13.6 kJ/m² Grade Count:10
 12.0 - 20.0 kJ/m²
@Thickness 3.00 - 3.20 mm
5.71 - 9.52 ft-lb/in²
@Thickness 0.118 - 0.126 in
Average value: 13.6 kJ/m² Grade Count:10
Izod Impact, Unnotched (ISO) NBNBGrade Count:4
 10.0 kJ/m² - NB
@Temperature -30.0 - -30.0 °C
4.76 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:2
 10.0 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.76 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:3
 10.0 - 10.0 kJ/m²
@Thickness 4.00 - 4.00 mm
4.76 - 4.76 ft-lb/in²
@Thickness 0.157 - 0.157 in
Average value: 10.0 kJ/m² Grade Count:3
Charpy Impact Unnotched 7.00 J/cm² - NB33.3 ft-lb/in² - NBAverage value: 7.00 J/cm² Grade Count:36
 1.40 J/cm² - NB
@Temperature -60.0 - -30.0 °C
6.66 ft-lb/in² - NB
@Temperature -76.0 - -22.0 °F
Average value: 1.40 J/cm² Grade Count:38
Charpy Impact, Notched 0.900 - 11.8 J/cm²4.28 - 56.2 ft-lb/in²Average value: 6.42 J/cm² Grade Count:31
 1.10 - 1.80 J/cm²
@Temperature -30.0 - -30.0 °C
5.24 - 8.57 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.36 J/cm² Grade Count:24
 1.20 - 1.80 J/cm²
@Temperature -30.0 - -30.0 °C
5.71 - 8.57 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.36 J/cm² Grade Count:10
 1.20 - 1.80 J/cm²
@Thickness 3.00 - 3.00 mm
5.71 - 8.57 ft-lb/in²
@Thickness 0.118 - 0.118 in
Average value: 1.36 J/cm² Grade Count:10
Gardner Impact 36.2 J26.7 ft-lbAverage value: 36.2 J Grade Count:3
Puncture Energy 50.0 - 65.0 J36.9 - 47.9 ft-lbAverage value: 58.9 J Grade Count:14
 55.0 - 75.0 J
@Temperature -30.0 - -30.0 °C
40.6 - 55.3 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 66.4 J Grade Count:14
Tensile Creep Modulus, 1 hour 2200 MPa319000 psiAverage value: 2200 MPa Grade Count:13
Tensile Creep Modulus, 1000 hours 1900 MPa276000 psiAverage value: 1900 MPa Grade Count:13
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 1.00e+17 ohm-cm1000 - 1.00e+17 ohm-cmAverage value: 1.00e+16 ohm-cm Grade Count:56
Surface Resistance 10000 - 1.00e+16 ohm10000 - 1.00e+16 ohmAverage value: 6.35e+15 ohm Grade Count:52
Dielectric Constant 2.70 - 3.172.70 - 3.17Average value: 3.01 Grade Count:45
Dielectric Strength 15.0 - 36.0 kV/mm380 - 914 kV/inAverage value: 28.6 kV/mm Grade Count:45
Dissipation Factor 0.000500 - 0.04000.000500 - 0.0400Average value: 0.00607 Grade Count:44
Arc Resistance 120 sec120 secAverage value: 120 sec Grade Count:6
Comparative Tracking Index 100 - 400 V100 - 400 VAverage value: 214 V Grade Count:20
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.650 - 70.2 µm/m-°C0.361 - 39.0 µin/in-°FAverage value: 64.9 µm/m-°C Grade Count:63
CTE, linear, Transverse to Flow 65.0 - 70.0 µm/m-°C36.1 - 38.9 µin/in-°FAverage value: 66.3 µm/m-°C Grade Count:30
Specific Heat Capacity 1.17 - 1.70 J/g-°C0.280 - 0.406 BTU/lb-°FAverage value: 1.54 J/g-°C Grade Count:9
Thermal Conductivity 0.173 - 0.210 W/m-K1.20 - 1.46 BTU-in/hr-ft²-°FAverage value: 0.199 W/m-K Grade Count:43
Melting Point 220 - 315 °C428 - 599 °FAverage value: 282 °C Grade Count:9
Maximum Service Temperature, Air 115 - 135 °C239 - 275 °FAverage value: 122 °C Grade Count:9
Hot Ball Pressure Test 115 - 141 °C239 - 286 °FAverage value: 136 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 127 - 147 °C261 - 297 °FAverage value: 138 °C Grade Count:62
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 170 °C176 - 338 °FAverage value: 128 °C Grade Count:82
Vicat Softening Point 114 - 155 °C237 - 311 °FAverage value: 147 °C Grade Count:64
Minimum Service Temperature, Air -60.0 - -40.0 °C-76.0 - -40.0 °FAverage value: -46.7 °C Grade Count:9
Glass Transition Temp, Tg 141 - 150 °C286 - 302 °FAverage value: 147 °C Grade Count:15
UL RTI, Electrical 75.0 - 130 °C167 - 266 °FAverage value: 114 °C Grade Count:16
UL RTI, Mechanical with Impact 75.0 - 125 °C167 - 257 °FAverage value: 108 °C Grade Count:16
UL RTI, Mechanical without Impact 75.0 - 130 °C167 - 266 °FAverage value: 114 °C Grade Count:16
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:56
Flash Point 450 - 560 °C842 - 1040 °FAverage value: 510 °C Grade Count:11
Oxygen Index 25.0 - 43.0 %25.0 - 43.0 %Average value: 29.3 % Grade Count:22
Glow Wire Test 750 - 960 °C1380 - 1760 °FAverage value: 885 °C Grade Count:27
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.59 - 1.591.59 - 1.59Average value: 1.59 Grade Count:28
Haze 0.500 - 1.00 %0.500 - 1.00 %Average value: 0.853 % Grade Count:17
Transmission, Visible 0.000 - 94.0 %0.000 - 94.0 %Average value: 70.4 % Grade Count:47
UV Transmittance 51.0 - 88.0 %51.0 - 88.0 %Average value: 74.3 % Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 310 °C500 - 590 °FAverage value: 288 °C Grade Count:13
Melt Temperature 250 - 343 °C482 - 650 °FAverage value: 302 °C Grade Count:31
Mold Temperature 60.0 - 120 °C140 - 248 °FAverage value: 83.6 °C Grade Count:42
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:21
Drying Temperature 100 - 124 °C212 - 255 °FAverage value: 119 °C Grade Count:19
Vent Depth 0.00127 cm0.000500 inAverage value: 0.00127 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Overview of materials for Polycarbonate, Impact Modified
Overview of materials for Acrylic, Extruded

O3101 / 78120

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.