MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sterigenics Raprex® R100D Branched High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Applications: Extrusion

RAPREX® R100D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched structure. It is a thermoplastic resin and is fully recyclable. Due to its broad molecular weight distribution and melt strength, RAPREX® R100D is used for pipes, extruded profiles, sheet and large blow molded articles. Raprex® R100D contains a robust stabilization package providing excellent melt stability as well as long-term heat aging.

Information provided by Sterigenics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
Melt Index of Compound 0.26 g/10 min
@Load 10.0 kg,
Temperature 190 °C
0.26 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.9 MPa2450 psiASTM D638
Tensile Strength, Yield 28.6 MPa4150 psiASTM D638
Elongation at Break 43 %43 %ASTM D638
Elongation at Yield 14 %14 %ASTM D638
Flexural Modulus 0.869 GPa126 ksiASTM D790
Izod Impact, Notched 1.20 J/cm2.25 ft-lb/inPartial Break; ASTM D256
 0.700 J/cm
@Temperature -40.0 °C
1.31 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 7194 High Density Polyethylene, Specialty Extrusion Resin
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade
Techmer ES HiFill FR® HDPE E FR

PRAPREX1 / 65277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.