MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Total 7194 High Density Polyethylene, Specialty Extrusion Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes:
  • Medium molecular weight
  • Narrow molecular weight distribution
  • Designed for high speed orientation
  • USP Class VI compliant

Applications:

  • Monofilament
  • Slit tape
  • Woven and knitted fabrics
  • Specialty films

Information provided by Total Petrochemicals.

Key Words: Designed for high speed orientation
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ASTM D792
Melt Flow  0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 1.9 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.9 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.1 MPa3200 psiASTM D638
Elongation at Break >= 500 %>= 500 %ASTM D638
Flexural Modulus 0.793 GPa115 ksiASTM D790
2% Secant Modulus 0.689 GPa100 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM D3417
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
processExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bayport Polymers Baystar™ 7195 High Density Polyethylene, Specialty Extrusion Resin
Overview of materials for High Density Polyethylene (HDPE), Extruded
Sterigenics Raprex® R100D Branched High Density Polyethylene
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade
Mitsubishi Chemical Advanced Materials TIVAR™ UV UHMW-PE, Natural & Colored Except Black

PTOTAL748 / 130473

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.