MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cupronickel 75-25, UNS C71300 Copper Coinage Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: This alloy is used primarily in coins. The hard rolled alloy creates clean blanks and the annealed alloy allows a good rendition of the coins features.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 69Hard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
Tensile Strength, Ultimate 52000 psiAnnealed
 78000 psiHard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
Tensile Strength, Yield 15000 psiAnnealed
Elongation at Break 11 %Hard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
 40 %Annealed
Tensile Modulus 2.20e+7 psi(C71500 Annealed)
Poissons Ratio 0.325(C71500 Annealed)
Machinability 20 %Based on Free cutting brass = 100%
Shear Modulus 8300 ksi(C71500 Annealed)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000287 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 228 BTU-in/hr-ft²-°F
Melting Point 2120 - 2240 °F
Solidus 2120 °F
Liquidus 2240 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 71.25 - 76.5 %As Remainder
Iron, Fe <= 0.20 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 1.0 %
Nickel, Ni 23.5 - 26.5 %
Zinc, Zn <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C70250, TM00 Temper strip
Copper nickel 30%, UNS C71500
Copper, UNS C73500
Copper nickel 20%, UNS C71000, H01 Temper flat products
Copper nickel 20%, UNS C71000

MC71300b1 / 11743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.