Description: Pro-fax™ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of properties and is suited for injection molding or extrusion applications. Pro-fax™ SD183 resin has a UL yellow card RTI of 65°C and a flame rating of UL94HB; these apply to all colors at a minimum thickness of 0.043 inches. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Appliances Information provided by Basell. |