MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: Injection Molding

Key Features: resistant to aging at high temperatures in both wet and dry environments, good cold impact resistance, excellent dimensional stability, FDA acceptable,

Applications: appliances, automotive under-the-hood appliances

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax 7624 medium impact polypropylene copolymer resin is highly resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of properties and is used for injection molding applications. It has a UL yellow card RTI, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Yield 9.0 %9.0 %ASTM D638
Flexural Modulus, 1% Secant 1200 MPa174000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256A
Impact Test 28.0 J
@Temperature -29.0 °C
20.7 ft-lb
@Temperature -20.2 °F
Montell drop weight impact strength
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
UL RTI, Mechanical with Impact 105 °C
@Thickness >=1.47 mm
221 °F
@Thickness >=0.0580 in
Flammability, UL94 HB
@Thickness >=1.47 mm
HB
@Thickness >=0.0580 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHN-230 Polypropylene Impact Copolymer

PMO186 / 53551

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.