MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe Double Six™ ASTM M2 High Speed Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: DOUBLE SIX (M2) is a tungsten-molybdenum high speed steel with a well balanced composition suitable for a wide variety of applications. World wide, the M2 type is by far the most popular high speed steel having replaced T1 high speed in most applications because of its superior properties and relative economy. Typical applications for Double Six high speed steel include twist drills, taps, milling cutters, reamers, broaches, saws, and knives.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.14 g/cc8.14 g/cc
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6464Oil Quenched from 1121°C
 64.564.5Oil Quenched from 1232°C
 6666Oil Quenched from 1177°C
Modulus of Elasticity 207 GPa30000 ksi
Machinability 50 - 60 %50 - 60 %1% Carbon Steel
Izod Impact Unnotched 51.5 J38.0 ft-lbOil Quenched at 1232°C; 482°C Temper Temperature
 55.6 J41.0 ft-lbOil Quenched at 1232°C; 545°C Temper Temperature
 56.9 J42.0 ft-lbOil Quenched at 1232°C; 622°C Temper Temperature
 56.9 J42.0 ft-lbOil Quenched at 1177°C; 482°C Temper Temperature
 66.4 J49.0 ft-lbOil Quenched at 1177°C; 622°C Temper Temperature
 96.3 J71.0 ft-lbOil Quenched at 1177°C; 566°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.95 µm/m-°C
@Temperature 21.0 - 204 °C
6.083 µin/in-°F
@Temperature 69.8 - 399 °F
 12.54 µm/m-°C
@Temperature 21.0 - 358 °C
6.967 µin/in-°F
@Temperature 69.8 - 676 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 749 °C1380 °FCritical Temperaure Ar3
 777 °C1430 °FCritical Temperaure Ar1
 832 °C1530 °FCritical Temperaure Ac1
 877 °C1610 °FCritical Temperaure Ac3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.85 %0.85 %
Chromium, Cr 4.15 %4.15 %
Iron, Fe 81.42 %81.42 %
Manganese, Mn 0.28 %0.28 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.30 %0.30 %
Tungsten, W 6.15 %6.15 %
Vanadium, V 1.85 %1.85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
Crucible Steel Rex M2 High Speed Steel
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Crucible Steel PM M2 Tool Steel
Latrobe HS-29XL™ ASTM M2-HC High Speed Steel

NTIMK062 / 19409

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.