MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) RHODAFAC® RS 710 D Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODAFAC® RS 710 D is a dispersing, emulsifying and wetting agent. Excellent dispersing properties. Diluted in water to facilitate use in applications.

Chemical Name: Complex organic phosphate ester, acid form

CAS No: 9046-01-9, 78330-21-9

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 29 - 31 %29 - 31 %CEM, 30% Power; RP-0528
 
Chemical PropertiesMetricEnglishComments
Acid Value 17.5 - 21.517.5 - 21.5KOH to first Infl. Pt; RP-0427
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear LiquidRP-0064
Content<5.4%Nonionic, RP-0351

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/710 Polyolefin
Solvay RHODASURF® DA-630 E Surfactant
Solvay RHODASURF® BC-720 Surfactant
Solvay RHODASURF® BC-610 Surfactant
Solvay RHODASURF® AAE-10 Surfactant

PSOLVAY769 / 218497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.