MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODASURF® BC-720 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Rhodasurf BC-720/E is non ionic low foaming agent for textile, processing and alkaline spray cleaners. Emulsification for Silicones, agricultural chemicals and petroleum oils.

Chemical Name: TRIDECYL ALCOHOL, ETHOXYLATED

CAS: 78330-21-9

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: Soluble in Water; Dispersible in alcohol, mineral oil, and acetone; Soluble in toluene.

Applications: RHODASURF© BC-720 is useful as an intermediate in the manufacture of high foaming anionic surfactants, such as water-soluble sulfate esters. RHODASURF© BC-720 is an oil soluble detergent / dispersing agent for petroleum hydrocarbons. RHODASURF© BC-720 is one of a series of Rhodia tridecyl alcohol ethoxylates with different HLBs. The products in the RHODASURF© BC series are made with a range of hydrophobe to ethylene oxide ratios allowing users to select a product with specific solubility characteristics for their system.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.5 - 8.56.5 - 8.510% Solution
 
Thermal PropertiesMetricEnglishComments
Pour Point 18.0 - 20.0 °C64.4 - 68.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy LiquidRP-0064, at 50°C
 Cloudy, Free Flowing LiquidRP-0064, at 25°C
Cloud point58-68°C1% Solution, RP-0124
Color<100APHA, RP-0134
HLB number13.8
Neutralization Number<0.5 mg KOH/gpH 7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODASURF® BC-840 Surfactant
Solvay RHODASURF® 870 Surfactant
Solvay RHODASURF® 91-6 Surfactant
Solvay RHODASURF® BC-610 Surfactant
Solvay RHODASURF® BC-630 Surfactant

WRHOD433 / 137664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.