MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ FC 2145 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Fluoroelastomer FC 2145 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FC 2145 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability
  • Composition: di-polymer of vinylidene fluoride and hexafluoropropylene
  • Low viscosity gumstock without incorporated curatives
  • Process targets: injection and transfer molding, extrusion, calendering and coatings
  • FC 2145 is amine or bisphenol curable

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Mooney Viscosity 28
@Temperature 121 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 1765 psiPress Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 184 %Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D4645
100% Modulus 0.805 ksi
@Strain 100 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 16 %
@Temperature 200 °C,
Time 252000 sec
Method B, -214 O-rings; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature -18.0 °CTR10; ASTM D1329
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 65.9 %
 
Descriptive Properties
ColorStraw
MH, Maximum Torque18.9 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque0.8 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
SolubilityKetones and Esters
t`50, Time to 50% cure2.4 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure 3.5 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min 1.9 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
Overview of materials for Nylon 6, Impact Grade

PDYNE098 / 34906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.