MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik SANMAC SAF 2205 Hollow Bar
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel

Material Notes: Sandvik SANMAC SAF 2205™ is a duplex stainless steel (austenitic-ferritic). It is characterized by:
  • excellent machinability
  • high resistance to stress corrosion cracking in chloride-bearing environments
  • high resistance to stress corrosion cracking in environments containing hydrogen sulphide
  • high resistance to general corrosion, pitting and crevice corrosion
  • high mechanical strength – roughly twice the proof strength of austenitic stainless steels
  • good hot-working properties
  • high resistance to erosion corrosion and corrosion fatigue
  • physical properties that offer design advantages
  • good weldability
  • Information provided by Sandvik

    UNS S31803, S32205; EN 1.4462

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.80 g/cc0.282 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell C <= 28<= 28
    Tensile Strength, Ultimate 660 - 880 MPa95700 - 128000 psi20 mm wall thickness
     >= 560 MPa
    @Temperature 300 °C
    >= 81200 psi
    @Temperature 572 °F
     >= 630 MPa
    @Temperature 100 °C
    >= 91400 psi
    @Temperature 212 °F
    Tensile Strength, Yield  >= 450 MPa
    @Strain 0.2 %
    >= 65300 psi
    @Strain 0.2 %
    20 mm wall thickness
     >= 500 MPa
    @Strain 1 %
    >= 72500 psi
    @Strain 1 %
    20 mm wall thickness
     >= 310 MPa
    @Strain 0.2 %,
    Temperature 300 °C
    >= 45000 psi
    @Strain 0.2 %,
    Temperature 572 °F
     >= 340 MPa
    @Strain 1 %,
    Temperature 300 °C
    >= 49300 psi
    @Strain 1 %,
    Temperature 572 °F
     >= 370 MPa
    @Strain 0.2 %,
    Temperature 100 °C
    >= 53700 psi
    @Strain 0.2 %,
    Temperature 212 °F
     >= 420 MPa
    @Strain 1 %,
    Temperature 100 °C
    >= 60900 psi
    @Strain 1 %,
    Temperature 212 °F
    Elongation at Break >= 25 %>= 25 %2", 20 mm wall thickness
     >= 25 %>= 25 %20 mm wall thickness
    Modulus of Elasticity 200 GPa29000 ksi
     180 GPa
    @Temperature 300 °C
    26100 ksi
    @Temperature 572 °F
     194 GPa
    @Temperature 100 °C
    28100 ksi
    @Temperature 212 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  13.0 µm/m-°C
    @Temperature 30.0 - 100 °C
    7.22 µin/in-°F
    @Temperature 86.0 - 212 °F
     13.5 µm/m-°C
    @Temperature 30.0 - 200 °C
    7.50 µin/in-°F
    @Temperature 86.0 - 392 °F
     14.5 µm/m-°C
    @Temperature 30.0 - 400 °C
    8.06 µin/in-°F
    @Temperature 86.0 - 752 °F
    Specific Heat Capacity  0.480 J/g-°C
    @Temperature 20.0 °C
    0.115 BTU/lb-°F
    @Temperature 68.0 °F
     0.530 J/g-°C
    @Temperature 200 °C
    0.127 BTU/lb-°F
    @Temperature 392 °F
     0.590 J/g-°C
    @Temperature 400 °C
    0.141 BTU/lb-°F
    @Temperature 752 °F
    Thermal Conductivity  14.0 W/m-K
    @Temperature 20.0 °C
    97.2 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     17.0 W/m-K
    @Temperature 200 °C
    118 BTU-in/hr-ft²-°F
    @Temperature 392 °F
     20.0 W/m-K
    @Temperature 400 °C
    139 BTU-in/hr-ft²-°F
    @Temperature 752 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C <= 0.030 %<= 0.030 %
    Chromium, Cr 21.5 %21.5 %
    Iron, Fe 67.6 %67.6 %As Balance
    Manganese, Mn 2.0 %2.0 %
    Molybdenum, Mo 3.2 %3.2 %
    Nickel, Ni 4.5 %4.5 %
    Nitrogen, N 0.17 %0.17 %
    Phosphorus, P <= 0.030 %<= 0.030 %
    Silicon, Si 1.0 %1.0 %
    Sulfur, S <= 0.015 %<= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sandvik SAF 2205 Billet
    Sandvik SANMAC SAF 2205 Bar Steel
    Sandvik SANMAC SAF 2205 Billet
    MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel
    Sandvik SAF 2205 Precision Wire

    NSANDV193 / 19087

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.