MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil C4LL 3625.85 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C4LL 3625 Series are ethylene 1-butene linear low density polyethylene resins with increased stiffness and a higher melt index. These resins can be used alone or as a component in blown or cast packaging and industrial film.

Availability: Latin America, North America

Additive:

  • Antiblock: No
  • Slip: 400 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Bread Bags
  • Cast Film
  • Food packaging
  • Packaging Films
  • Paper Overwrap
  • Zipper Bag

Information provided by ExxonMobil

Key Words: LLDPE LL 1236.85
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ExxonMobil method
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Slip Level 400 ppm400 ppm
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 26.7 N6.00 lb (f)ExxonMobil Method
Film Tensile Strength at Yield, MD 10.3 MPa1500 psiASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa1500 psiASTM D882
Film Elongation at Break, MD 530 %530 %ASTM D882
Film Elongation at Break, TD 810 %810 %ASTM D882
Puncture Energy 1.58 J1.17 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 30 g30 gASTM D1922
Elmendorf Tear Strength TD 280 g280 gASTM D1922
Dart Drop Test <= 60.0 g<= 0.132 lbASTM D1709A
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psiASTM D882
1% Secant Modulus, MD 207 MPa30000 psiASTM D882
1% Secant Modulus, TD 228 MPa33000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 100 °C212 °FExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.3 %2.3 %ASTM D1003
Gloss 92 %92 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force7 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
ExxonMobil LL 5100.09 Compounding Resin
ExxonMobil LL 1002.09 Blown Film Resin
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin

PEX99155 / 175391

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.