MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

PTS PCA-2201NH-V Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: This is a Non-Halogenated Flame Retardant. Uses: Electronic and telecommunications enclosures, computer equipment, appliances

Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Linear Mold Shrinkage 0.004 - 0.006 cm/cm0.004 - 0.006 in/inASTM D955
Melt Flow  12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
12 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
13 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa
@Thickness 3.17 mm
8700 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 65 %
@Thickness 3.17 mm
65 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 88.9 MPa
@Thickness 3.17 mm
12900 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.69 GPa
@Thickness 3.17 mm
390 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 5.87 J/cm
@Thickness 3.17 mm
11.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm457 kV/in
Comparative Tracking Index >= 600 V>= 600 VPLC 0
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness 1.50 mm
15 - 30 sec
@Thickness 0.0591 in
PLC 3
 15 - 30 sec
@Thickness 2.50 mm
15 - 30 sec
@Thickness 0.0984 in
PLC 3
 30 - 60 sec
@Thickness 3.00 mm
30 - 60 sec
@Thickness 0.118 in
PLC 2
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
PLC 1
 60 - 120 arcs
@Thickness 2.50 mm
60 - 120 arcs
@Thickness 0.0984 in
PLC 1
 60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
PLC 1
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
@Thickness 3.17 mm
205 °F
@Thickness 0.125 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 3.17 mm
185 °F
@Thickness 0.125 in
ASTM D648
Vicat Softening Point 110 °C230 °F
UL RTI, Electrical 60.0 °C140 °F
UL RTI, Mechanical with Impact 60.0 °C140 °F
UL RTI, Mechanical without Impact 60.0 °C140 °F
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
all colors; UL file E155285
 5VB
@Thickness 2.00 mm
5VB
@Thickness 0.0787 in
all colors; UL file E155285
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in
 5VA
@Thickness 3.0 mm
5VA
@Thickness 0.12 in
all colors; UL file E155285
Glow Wire Ignition Temperature  700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  925 °C
@Thickness 1.50 mm
1700 °F
@Thickness 0.0591 in
IEC 60695-2-12
 925 °C
@Thickness 2.00 mm
1700 °F
@Thickness 0.0787 in
IEC 60695-2-12
 950 °C
@Thickness 3.00 mm
1740 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 266 °C450 - 511 °F
Middle Barrel Temperature 246 - 274 °C475 - 525 °F
Front Barrel Temperature 246 - 288 °C475 - 550 °F
Melt Temperature 246 - 288 °C475 - 550 °F
Mold Temperature 57.2 - 85.0 °C135 - 185 °Fsurface
Drying Temperature 87.8 °C
@Time 10800 - 14400 sec
190 °F
@Time 3.00 - 4.00 hour
Injection Pressure 68.9 - 110 MPa10000 - 16000 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Screw Speed 25 - 75 rpm25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Lotte Advanced Materials Infino® NH-1027HF PC/ABS, Unreinforced FR
Trinseo EMERGE™ PC/ABS 7700 NA Polycarbonate Resin

PZ9PU42r5 / 143022

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.