Sandvik 10R19 is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterized by: high creep strength very good resistance to isothermal and, above all, cyclic oxidationvery good resistance to combustion gasesgood structural stability at high temperatures good weldabilitythe grade can be used at temperatures up to about 1150°C (2100°F). Information provided by Sandvik UNS S30815; EN 1.4835 |