MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik F45-10R19 Billet
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik 10R19 is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterized by:
  • high creep strength
  • very good resistance to isothermal and, above all, cyclic oxidation
  • very good resistance to combustion gases
  • good structural stability at high temperatures
  • good weldability
  • the grade can be used at temperatures up to about 1150°C (2100°F).
  • Information provided by Sandvik

    UNS S30815; EN 1.4835

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.080 %0.080 %
    Chromium, Cr 21 %21 %
    Iron, Fe 65.5 %65.5 %As Balance
    Manganese, Mn 0.60 %0.60 %
    Nickel, Ni 11 %11 %
    Nitrogen, N 0.17 %0.17 %
    Phosphorus, P <= 0.040 %<= 0.040 %
    Silicon, Si 1.6 %1.6 %
    Sulfur, S <= 0.030 %<= 0.030 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition
    Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel
    Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel
    Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
    Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel

    NSANDV173 / 19067

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.