MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crucible Steel CPM® 1V® High Alloy Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel; Tool Steel

Material Notes: CPM 1V is a medium carbon, high alloy tool steel which exhibits high toughness combined with high heat resistance. It is suited for both hot or cold applications which demand high impact toughness and also require moderate wear resistance.

The CPM (Crucible Particle Metallurgy) process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 187Annealed
Hardness, Rockwell C 57 - 59
Modulus of Elasticity 207 GPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 21.88 W/m-K
 23.88 W/m-K
@Temperature 100 °C
 25.8 W/m-K
@Temperature 300 °C
 26.76 W/m-K
@Temperature 400 °C
 28.09 W/m-K
@Temperature 540 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.55 %
Chromium, Cr 4.5 %
Iron, Fe 89.05 %As Remainder
Molybdenum, Mo 2.75 %
Tungsten, W 2.15 %
Vanadium, V 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crucible Steel CPM® 3V® Tool Steel
Crucible Steel CPM® 9V® Tool Steel
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
Crucible Steel CPM® S30V® Stainless Steel

NCRUC000 / 15993

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.