MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel CPM® 9V® Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced properties permit CPM 9V to perform well in problem applications where high carbon, high chromium tool steels, such as CPM 10V or the high speed steels, lack sufficient toughness or heat check resistance, or where lower alloy tool steels and hot work tool steels lack sufficient wear resistance.

The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.455 g/cc0.2693 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 223 - 255223 - 255Annealed
Hardness, Rockwell C 54 - 5654 - 56
Modulus of Elasticity 221 GPa32100 ksi
Flexural Strength 4136 MPa599900 psiHardening Temperature- 1120°C, Tempering Temperature- 540°C
 4177 MPa605800 psiHardening Temperature- 1175°C, Tempering Temperature- 550°C
Charpy Impact 35.0 J25.8 ft-lbHardening Temperature- 1175°C; Tempering Temperature- 550°C
 63.0 J46.5 ft-lbHardening Temperature- 1120°C; Tempering Temperature- 540°C
 99.0 J73.0 ft-lbHardening Temperature- 1065°C; Tempering Temperature- 595°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.07 µm/m-°C
@Temperature 20.0 - 90.0 °C
6.150 µin/in-°F
@Temperature 68.0 - 194 °F
 11.18 µm/m-°C
@Temperature 20.0 - 200 °C
6.211 µin/in-°F
@Temperature 68.0 - 392 °F
 11.61 µm/m-°C
@Temperature 20.0 - 430 °C
6.450 µin/in-°F
@Temperature 68.0 - 806 °F
Thermal Conductivity 20.48 W/m-K142.1 BTU-in/hr-ft²-°F
 21.6 W/m-K
@Temperature 100 °C
150 BTU-in/hr-ft²-°F
@Temperature 212 °F
 25.25 W/m-K
@Temperature 300 °C
175.2 BTU-in/hr-ft²-°F
@Temperature 572 °F
 25.81 W/m-K
@Temperature 500 °C
179.1 BTU-in/hr-ft²-°F
@Temperature 932 °F
 26.08 W/m-K
@Temperature 540 °C
181.0 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.9 %1.9 %
Chromium, Cr 5.25 %5.25 %
Iron, Fe 82.45 %82.45 %As Remainder
Molybdenum, Mo 1.3 %1.3 %
Vanadium, V 9.1 %9.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® 3V® Tool Steel
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
Crucible Steel CPM® 1V® High Alloy Tool Steel
Crucible Steel CPM® S90V® (420V®) Tool Steel
Crucible Steel CPM® 15V® Tool Steel

NCRUC002 / 15995

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.