MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel CPM® 10V® (AISI A11) Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistance while maintaining toughness and fabrication characteristics comparable to D2 and M2. Since its introduction in 1978, CPM 10V has become recognized world-wide and sets the standard for highly wear resistant industrial tooling. Its exceptional wear resistance and good toughness make it an excellent candidate to replace carbide and other highly wear resistant materials in cold work tooling applications, particularly where tool toughness is a problem or where cost effectiveness can be demonstrated.

The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.418 g/cc0.2680 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 255 - 277255 - 277Annealed
Hardness, Rockwell C 6060
Modulus of Elasticity 221 GPa32100 ksi
Flexural Strength 4322 MPa626900 psiHardening Temperature- 1175°C, Tempering Temperature- 540°C
 4377 MPa634800 psiHardening Temperature- 1120°C, Tempering Temperature- 550°C
Charpy Impact 20.0 J14.8 ft-lbHardening Temperature- 1175°C; Tempering Temperature- 540°C
 30.0 J22.1 ft-lbHardening Temperature- 1120°C; Tempering Temperature- 550°C
 35.0 J25.8 ft-lbHardening Temperature- 1065°C; Tempering Temperature- 550°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.7 µm/m-°C
@Temperature 21.0 - 93.0 °C
5.94 µin/in-°F
@Temperature 69.8 - 199 °F
 11.1 µm/m-°C
@Temperature 21.0 - 260 °C
6.17 µin/in-°F
@Temperature 69.8 - 500 °F
 12.3 µm/m-°C
@Temperature 21.0 - 593 °C
6.83 µin/in-°F
@Temperature 69.8 - 1100 °F
Thermal Conductivity 20.39 W/m-K141.5 BTU-in/hr-ft²-°F
 21.54 W/m-K
@Temperature 100 °C
149.5 BTU-in/hr-ft²-°F
@Temperature 212 °F
 24.85 W/m-K
@Temperature 300 °C
172.5 BTU-in/hr-ft²-°F
@Temperature 572 °F
 26.3 W/m-K
@Temperature 500 °C
183 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.45 %2.45 %
Chromium, Cr 5.25 %5.25 %
Iron, Fe 81.25 %81.25 %As Remainder
Molybdenum, Mo 1.3 %1.3 %
Vanadium, V 9.75 %9.75 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® 15V® Tool Steel
AISI Type S7 Tool Steel (UNS T41907)
Carpenter Micro-Melt® 10 Tough Treated Tool Steel (AISI A11)
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)

NCRUC003 / 15996

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.