MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: This resin is a hexene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It contains of slip & antiblock additives. This product meets US FDA 21 CFR 177.1520.

Applications: Bags; Film; Industrial Applications; Liners; Packaging.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Hexene Comonomer; Food Contact Acceptable; Toughness; High Impact Resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 1.0 g/10 min1.0 g/10 minASTM D1238
Antiblock Level 7000 ppm7000 ppm
Slip Level 1500 ppm1500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 690 %690 %ASTM D882
Elmendorf Tear Strength MD 380 g380 gASTM D1922
Elmendorf Tear Strength TD 600 g600 gASTM D1922
Dart Drop Test 150 g0.331 lbASTM D1709
Film Tensile Strength at Break, MD 31.37 MPa4550 psiASTM D882
Film Tensile Strength at Break, TD 23.44 MPa3400 psiASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
Bamberger Polymers Bapolene® 270F Low Density Polyethylene Film Extrusion Resin
Bamberger Polymers Bapolene® 2292 Polyethylene Film Grade
Bamberger Polymers Bapolene® 222F Polyethylene, Film Grade

PBP1136 / 193452

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.