MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bamberger Polymers Bapolene® 2292 Polyethylene Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.

Applications: Closures; Household Goods; Lids.

All data is based on molded plaques.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Butene Comonomer; Food Contact Acceptable; Good Stiffness; Good Toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D-1505
Melt Flow 50 g/10 min50 g/10 minASTM D-1228
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 10.3 MPa1500 psiASTM D-638
Elongation at Break 90 %90 %ASTM D-638
Flexural Modulus, 1% Secant 345 MPa50000 psiASTM D-790
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 959S Linear Low Density Polyethylene (LDPE)
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade
Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin

PBP1119 / 83166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.