MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® FG70G30HSR2 BK309 PA66-GF30  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Heat Stabilized, Polyamide 66 Developed for Food Contact Applications

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³DAM; ISO 1183
Melt Density 1.20 g/cc
@Temperature >=263 °C
0.0434 lb/in³
@Temperature >=505 °F
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi50% RH; ISO 527-1/-2
 200 MPa29000 psiDAM; ISO 527-1/-2
Elongation at Break 3.3 %3.3 %DAM; ISO 527-1/-2
 5.0 %5.0 %50% RH; ISO 527-1/-2
Tensile Modulus 7.20 GPa1040 ksi50% RH; ISO 527-1/-2
 10.0 GPa1450 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.340.34DAM; ISO 527-1/-2
 0.350.3550%RH; ISO 527-1/-2
Charpy Impact Unnotched  7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 ohm1.00e+13 ohm50% RH; IEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 28.0 µm/m-°C15.6 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C52.8 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 2.22 J/g-°C
@Temperature >=263 °C
0.531 BTU/lb-°F
@Temperature >=505 °F
Melt
Thermal Conductivity 0.220 W/m-K
@Temperature >=263 °C
1.53 BTU-in/hr-ft²-°F
@Temperature >=505 °F
Melt
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FDAM; ISO 75-1/-2
Vicat Softening Point 209 °C408 °F50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 20.0 °C68.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 80.0 °C176 °F10°C/min; DAM; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 24 %24 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 305 °C545 - 581 °FInjection
 295 °C563 °FInjection Optimum
Mold Temperature 50.0 - 120 °C122 - 248 °FInjection
 100 °C212 °FInjection Optimum
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
Eff. thermal diffusivity6.85E-08 m²/s
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-GF30ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA66-GF30ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 70G30L NC010 PA66-GF30
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
Celanese Celstran® PA66-GF30-02 Nylon 66, 30% Glass Reinforced
Celanese Zytel® 70G30HSLR NC010 PA66-GF30
Celanese Zytel® 70G30HSLR BK099 PA66-GF30

PDSX5410 / 198050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.