MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications
Categories: Polymer; Adhesive

Material Notes: Description: Master Bond Polymer System UV15X-6MED-2 is a newly developed one component clear, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasion resistance. This high viscosity system can be used for bonding, sealing, coating and casting. Master Bond UV15X-6MED-2 offers excellent physical strength properties including high elongation, good resistance to severe environmental conditions as well as the ability to withstand thermal cycling and thermal and mechanical shock. The service temperature range is -80°F to +300°F. UV15X-6MED-2 bonds well to a variety of substrates including glass, various plastics such as polycarbonates and acrylics, selected rubbers, and metals. In addition, Master Bond UV15X-6MED-2 possesses excellent thermal and electrical insulation properties. UV15X-6MED-2 is 100% reactive and does not contain solvents or other volatiles. *Most importantly, UV15X-6MED-2 meets USP Class VI specifications. With commercially available UV lamps cures “on demand” can be effected in very short time periods i.e. 1 minute or less at ambient temperatures. For example, when curing the UV15X-6MED-2 in thinner sections (10 mils or less) with a 200 watt mercury vapor continuous light source emitting at 365 nm, UV15X-6MED will cure tack free within 10 seconds at 40 milliwatts of output per cm². UV15X-6MED-2 will cure in thickness greater than 1/8” thick although the cure is not quite as rapid as it would be in thinner sections. Master Bond Polymer System UV15X-6MED-2 is not air inhibited. No solvents or other volatiles are emitted during cure. Master Bond UV15X-6MED-2 contains an exceptionally active UV curing initiator which makes cures practical even with relatively low intensity UV light sources.

Product Advantages:

  • One component system; no mixing needed; ready to use as supplied
  • Exceptionally fast cure upon exposure to a UV light source at ambient temperatures
  • No air inhibition while curing; no special inert atmosphere required
  • 100% reactive; no volatiles emitted during cure
  • High physical strength properties; good electrical and thermal insulation characteristics
  • Excellent elongation; high impact strength; withstands thermal cycling and shock
  • Outstanding abrasion resistance
  • Good adhesion to many substrates especially glass and plastics
  • Good chemical resistance and weather ability
  • Meets USP Class VI specifications

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Viscosity >= 24000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25 - 30
Tensile Strength at Break 1600 psi
Elongation at Break >= 200 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -80.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5006
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Monthin original unopened container
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP3HTSMed Silver Filled, Medical Grade Epoxy
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Master Bond UV15X-2 One Component, Non-Yellowing UV Curable Adhesive
Master Bond UV15TK High Temperature Resistant One Component UV Curable System

PMASTB366 / 149613

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.