MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15TK High Temperature Resistant One Component UV Curable System
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Master Bond UV15TK is a moderate viscosity, epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is also completely free of any oxygen inhibition. Along with outstanding temperature resistance, UV15TK has superior physical properties and dimensional stability.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 8000 - 10000 cP
@Temperature 23.0 °C
8000 - 10000 cP
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Descriptive Properties
ColorSlight Amber; Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond UV15DC80Med One Component UV Curable Epoxy
Master Bond UV15X-6NM-2 One Component UV Curing Urethane Acrylate
Master Bond UV15X-6MED-2 UV Curable Compound for Medical Applications
Master Bond UV15X-5 One Component High Viscosity UV Curable System
Master Bond UV15X-2GT One Component, UV Curable Glob Top Compound

PMASTB128 / 52285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.