MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Dyneon™ FX 5914 Polymer Processing Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Fluoropolymer, TS

Material Notes: Dynamar FX 5914 is a free-flowing fluoropolymer processing additive (PPA) that is designed for use at very low levels to improve processing of thermoplastics. At the use levels (typically 200-1000 ppm) necessary to improve processing, it does not alter or detract from the good physical properties associated with high strength plastics.

Feature and Benefits

  • For use with basic polymers and additives
  • Applicable in engineering thermoplastics like nylon, polyester, PVC, polystyrene, and acrylic
  • Free-flowing fluoropolymer processing additive
  • For use at very low levels
  • Excellent thermal stability for high temperature processing
  • Reduces or eliminates die build-up
  • Speeds colorant changes
  • Lowers apparent melt viscosity
  • Reduces gel formation

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.76 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 195 - 215 °C
 
Descriptive Properties
Active Ingredients (%)100
ColorClear to off-white
FormAgglomerate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PA66 A 1000/517.01 IM Nylon 66
Toagosei America Aron Alpha® Industrial Krazy Glue™ 253TX Cyanoacrylate Adhesive
Toagosei America Aron Alpha® Industrial Krazy Glue™ 101 Cyanoacrylate Adhesive
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Taiwan Sheen Soon Sheenthane® AH-701 TPU for Hotmelt Adhesive

PDYNE158 / 34966

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.