MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blown film applications requiring outstanding sealability and toughness

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Thickness 31.8 microns1.25 mil
Melt Flow 1.2 g/10 min1.2 g/10 minExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 4.96 MPa720 psiASTM D882
Film Tensile Strength at Yield, TD 4.55 MPa660 psiASTM D882
Film Elongation at Break, MD 480 %480 %ASTM D882
Film Elongation at Break, TD 630 %630 %ASTM D882
Film Elongation at Yield, MD 9.4 %9.4 %ASTM D882
Film Elongation at Yield, TD 8.4 %8.4 %ASTM D882
Puncture Energy 7.74 J5.71 ft-lbExxonMobil Method
Elmendorf Tear Strength, MD 5.35 g/micron136 g/milASTM D1922
Elmendorf Tear Strength, TD 8.82 g/micron224 g/milASTM D1922
Dart Drop 41.89 g/micron1064 g/milASTM D1709A
Film Tensile Strength at Break, MD 73.50 MPa10660 psiASTM D882
Film Tensile Strength at Break, TD 73.84 MPa10710 psiASTM D882
1% Secant Modulus, MD 73.1 MPa10600 psiASTM D882
1% Secant Modulus, TD 77.2 MPa11200 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.6 °C204 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 79.0 °C174 °FExxonMobil Method
Vicat Softening Point 87.8 °C190 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %2.5 %ASTM D1003
Gloss 80 %80 %ASTM D2457
 
Descriptive Properties
Puncture Force17 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin

PEXB348 / 37653

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.