MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Electrodag® 440 AS EMC Coating
Categories: Other Engineering Material

Material Notes: Electrodag 440 AS is one of a series of Electrodag EMC coatings designed to provide electromagnetic compatibility (EMC) on cabinetry used for electronic equipment. It is a highly conductive nickel coating providing excellent shielding against radiated electromagnetic interference (EMI) and protection against electrostatic discharge (ESD). Electrodag 440 AS combines increased conductivity with improved economy; it offers improved ease of application and excellent stability to difficult environmental conditions such as high humidity or heat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.03 g/cc
Solids Content 69 - 71 %
Filler Content 69 - 71 %Nickel
Viscosity 4500 - 7000 cP
Thickness 50.0 - 75.0 microns
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.50 ohm
 
Processing PropertiesOriginal ValueComments
Cure Time 1200 - 1800 sec
 
Descriptive Properties
Adhesion5B (excellent)
Binder Systemthermoplastic resin
Conductive Filler TypeNickel
Material TypeReady-To-Use Formulation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cosmic Plastics CP7314 Epoxy Molding Compound
Henkel Acheson™ PM-460A Conductive Resin
Henkel Acheson™ PM-500™ Conductive Coating
Henkel Electrodag® 461 SS Conductive Ink
Henkel Electrodag® 965 SS Conductive Ink

PFLEXCM19 / 179421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.