MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Acheson™ PM-460A Conductive Resin
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: PM-460A is a dispersion of silver pigment in a thermoplastic resin system that rapidly dries to form a flexible conductive coating. It is designed to be applied by flexographic or rotogravure printing techniques. PM-460A can be applied to plastic as well as paper substrates. The coating will maintain its low resistance even after exposure to heat, cold and humid conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.34 g/cc0.0845 lb/in³
Solids Content 72 %72 %
Filler Content 72 %72 %Silver (Ag)
Viscosity 4000 cP4000 cP
Thickness 10.0 microns0.394 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.010 ohm0.010 ohm
 
Descriptive Properties
Binder Systemthermoplastic resin
Conductive Filler TypeSilver (Ag)
Material TypeDispersion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Electrodag® PD-056 Conductive Resin
Henkel Acheson™ PM-500™ Conductive Coating
Henkel Electrodag® 965 SS Conductive Ink
Henkel Electrodag® 461 SS Conductive Ink
Henkel Electrodag® 440 AS EMC Coating

PFLEXCM57 / 179459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.