MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI Type 440B Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Higher hardness than Type 440A.

Information provided by Chevron-Phillips Chemical Company, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.74 g/cc(for Stainless 410A0)
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 200 GPa(for Stainless 410A0)
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 24.2 W/m-K(for Stainless 410A0)
Melting Point 1400 - 1500 °C(for Stainless 410A0)
Solidus 1400 °C(for Stainless 410A0)
Liquidus 1500 °C(for Stainless 410A0)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.75 - 0.95 %
Chromium, Cr 16 - 18 %
Iron, Fe 82 %As remainder
Manganese, Mn <= 1.0 %
Molybdenum, Mo <= 0.75 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Type 440B Martensitic Stainless Steel, Annealed Bar, UNS S44003
440C Martensitic Stainless Steel (UNS S44004)
Type 440B Martensitic Stainless Steel Bar, Tempered at 315°C, UNS S44003
440A Martensitic Stainless Steel (UNS S44002)
410 Stainless Steel

MQ440B / 13213

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.