MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Gamma Radiation Resistant, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 - 1.17 g/cc0.0390 - 0.0423 lb/in³Average value: 1.13 g/cc Grade Count:13
Water Absorption 0.300 - 2.00 %0.300 - 2.00 %Average value: 0.709 % Grade Count:9
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm0.00300 - 0.00800 in/inAverage value: 0.00543 cm/cm Grade Count:7
Melt Flow 1.60 - 12.0 g/10 min1.60 - 12.0 g/10 minAverage value: 5.35 g/10 min Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 27.0 - 60.027.0 - 60.0Average value: 37.8 Grade Count:6
Tensile Strength, Ultimate 36.3 - 50.3 MPa5270 - 7300 psiAverage value: 43.2 MPa Grade Count:11
Elongation at Break 5.00 - 50.0 %5.00 - 50.0 %Average value: 24.0 % Grade Count:13
Elongation at Yield 3.60 - 4.50 %3.60 - 4.50 %Average value: 3.99 % Grade Count:7
Modulus of Elasticity 1.38 - 2.96 GPa200 - 430 ksiAverage value: 2.06 GPa Grade Count:13
Flexural Yield Strength 46.9 - 85.5 MPa6800 - 12400 psiAverage value: 64.8 MPa Grade Count:11
Flexural Modulus 1.65 - 2.45 GPa240 - 355 ksiAverage value: 2.08 GPa Grade Count:7
Izod Impact, Notched 0.320 - 1.23 J/cm0.600 - 2.30 ft-lb/inAverage value: 0.776 J/cm Grade Count:11
 0.42712 - 0.58729 J/cm
@Temperature 0.000 - 0.000 °C
0.80017 - 1.1002 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.534 J/cm Grade Count:3
 0.42712 - 0.58729 J/cm
@Diameter 6.35 - 6.35 mm
0.80017 - 1.1002 ft-lb/in
@Diameter 0.250 - 0.250 in
Average value: 0.534 J/cm Grade Count:3
Gardner Impact 3.05 - 7.34 J2.25 - 5.42 ft-lbAverage value: 5.20 J Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 - 100 µm/m-°C40.0 - 55.6 µin/in-°FAverage value: 88.4 µm/m-°C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 90.0 °C185 - 194 °FAverage value: 87.6 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 85.6 °C158 - 186 °FAverage value: 78.9 °C Grade Count:13
Vicat Softening Point 80.0 - 112 °C176 - 234 °FAverage value: 95.1 °C Grade Count:13
Flammability, UL94 HBHBGrade Count:7
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49 - 1.511.49 - 1.51Average value: 1.50 Grade Count:5
Haze 2.00 - 7.00 %2.00 - 7.00 %Average value: 4.29 % Grade Count:7
Yellow Index -1.00 - -0.300 %-1.00 - -0.300 %Average value: -0.440 % Grade Count:5
Transmission, Visible 80.0 - 91.0 %80.0 - 91.0 %Average value: 88.0 % Grade Count:13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 249 °C360 - 480 °FAverage value: 223 °C Grade Count:5
Mold Temperature 48.9 - 82.2 °C120 - 180 °FAverage value: 65.6 °C Grade Count:5
Drying Temperature 71.1 - 79.4 °C160 - 175 °FAverage value: 74.4 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cellulose Acetate, Molded
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylic, High Flow, Molded
Overview of materials for Acrylic, Impact Modified, Molded
Overview of materials for Acrylic, Extruded

O1308 / 77867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.