MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Cellulose Acetate, Molded
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 - 1.31 g/cc0.0455 - 0.0473 lb/in³Average value: 1.27 g/cc Grade Count:31
Water Absorption 1.90 - 7.00 %1.90 - 7.00 %Average value: 2.42 % Grade Count:22
Linear Mold Shrinkage 0.00200 - 0.00850 cm/cm0.00200 - 0.00850 in/inAverage value: 0.00411 cm/cm Grade Count:20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 31.0 - 11731.0 - 117Average value: 78.2 Grade Count:15
Tensile Strength, Ultimate 12.0 - 110 MPa1740 - 16000 psiAverage value: 38.3 MPa Grade Count:25
Tensile Strength, Yield 19.0 - 55.0 MPa2760 - 7980 psiAverage value: 33.0 MPa Grade Count:31
Elongation at Break 15.0 - 72.0 %15.0 - 72.0 %Average value: 31.0 % Grade Count:27
Elongation at Yield 3.10 - 4.00 %3.10 - 4.00 %Average value: 3.36 % Grade Count:8
Modulus of Elasticity 1.00 - 4.00 GPa145 - 580 ksiAverage value: 2.08 GPa Grade Count:10
Flexural Yield Strength 27.0 - 72.0 MPa3920 - 10400 psiAverage value: 48.5 MPa Grade Count:23
Flexural Modulus 0.0800 - 2.62 GPa11.6 - 380 ksiAverage value: 1.21 GPa Grade Count:23
Izod Impact, Notched 0.480 - 4.50 J/cm0.899 - 8.43 ft-lb/inAverage value: 2.06 J/cm Grade Count:23
 0.370 - 0.690 J/cm
@Temperature -40.0 - -40.0 °C
0.693 - 1.29 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.561 J/cm Grade Count:15
Charpy Impact Unnotched 16.5 J/cm² - NB78.5 ft-lb/in² - NBAverage value: 16.5 J/cm² Grade Count:9
 NB - NB
@Temperature -30.0 - -30.0 °C
NB - NB
@Temperature -22.0 - -22.0 °F
Grade Count:7
Charpy Impact, Notched 0.700 - 1.83 J/cm²3.33 - 8.71 ft-lb/in²Average value: 1.39 J/cm² Grade Count:9
 0.470 - 1.03 J/cm²
@Temperature -30.0 - -30.0 °C
2.24 - 4.90 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.613 J/cm² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm1.00e+13 - 1.00e+15 ohm-cmAverage value: 5.05e+14 ohm-cm Grade Count:5
Dielectric Constant 3.30 - 5.003.30 - 5.00Average value: 3.79 Grade Count:6
Dielectric Strength 11.0 - 18.7 kV/mm279 - 475 kV/inAverage value: 14.5 kV/mm Grade Count:6
Dissipation Factor 0.00380 - 0.1500.00380 - 0.150Average value: 0.0663 Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 - 180 µm/m-°C6.11 - 100 µin/in-°FAverage value: 81.0 µm/m-°C Grade Count:13
CTE, linear, Transverse to Flow 129 - 151 µm/m-°C71.7 - 83.9 µin/in-°FAverage value: 141 µm/m-°C Grade Count:7
Specific Heat Capacity 1.20 - 1.90 J/g-°C0.287 - 0.454 BTU/lb-°FAverage value: 1.48 J/g-°C Grade Count:6
Thermal Conductivity 0.160 - 0.360 W/m-K1.11 - 2.50 BTU-in/hr-ft²-°FAverage value: 0.252 W/m-K Grade Count:6
Melting Point 138 - 180 °C280 - 356 °FAverage value: 160 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 52.0 - 105 °C126 - 221 °FAverage value: 81.5 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 86.0 °C118 - 187 °FAverage value: 69.4 °C Grade Count:21
Vicat Softening Point 78.0 - 113 °C172 - 235 °FAverage value: 96.8 °C Grade Count:20
Glass Transition Temp, Tg 95.0 - 108 °C203 - 226 °FAverage value: 102 °C Grade Count:7
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46 - 1.491.46 - 1.49Average value: 1.48 Grade Count:6
Haze 1.40 - 8.50 %1.40 - 8.50 %Average value: 7.32 % Grade Count:6
Transmission, Visible 86.0 - 90.0 %86.0 - 90.0 %Average value: 89.3 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 225 °C347 - 437 °FAverage value: 197 °C Grade Count:6
Melt Temperature 202 - 250 °C396 - 482 °FAverage value: 226 °C Grade Count:14
Mold Temperature 38.0 - 71.0 °C100 - 160 °FAverage value: 54.4 °C Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Polycarbonate, Molded
Overview of materials for Acrylic, Extruded
Overview of materials for Acrylic, Impact Modified, Molded
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled

O1651 / 77885

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.