MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Torque Fluid SAE Grade 50
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Torque Fluid Torque Fluid is a high-performance multifunctional fluid developed for use in transmissions, final drives and hydraulic systems of off-highway equipment where a fluid meeting Caterpillar TO-4 performance requirements is specified. It provides substantially improved friction and antiwear performance compared with older API CD/TO-2 quality fluids, resulting in longer equipment life and reduced risk of field failure. The SAE 10W and 30 viscosity grades also are recommended for use in Allison off-highway heavy-duty automatic transmissions where a C-4 quality fluid is specified. Torque Fluid is formulated with state-of-the-art additive technology that provides improved deposit control, corrosion protection and load-carrying capacity for better equipment protection and more reliable operation. Its carefully optimized frictional properties prevent clutch slippage for smoother, more consistent transmission operation and also provide improved wet brake performance.

Applications:

  • Powershift transmissions, hydrostatic transmissions, torque converters, final drives and hydraulic systems of Caterpillar, Euclid, Komatsu and other off-highway construction and mining equipment
  • Heavy-duty automatic transmissions where the OEM specifies an Allison C-4 quality fluid
  • Heavy-duty manual and semi-automatic transmissions in trucksand buses where the OEM specifies a Caterpillar TO-4 quality fluid or a heavy-duty engine oil
Torque Fluid SAE 30 is OEM-approved for service fill in the following applications:
  • Allison TES-439, for off-highway applications (approval no.439-33432013)
Torque Fluid meets or exceeds the requirements of:
  • Caterpillar TO-4, TO-2(1)
  • Vickers (Eaton) M-2950-S
Torque Fluid is recommended for service fill in:
  • ZF torque converter transmissions in off-highway equipment where the OEM specifies a TE-ML 03C quality lubricant (SAE 10W, 30)
Features/Benefits:
  • Well-balanced frictional properties for efficient clutch operation and improved wet brake performance
  • Excellent oxidation resistance and thermal stability for long fluid life
  • High load-carrying capacity for protection of final drive gear sets
  • Excellent deposit control and wear protection
  • Protects yellow metals against corrosion
  • High shear stability
  • Compatible with a wide variety of seals and friction materials
  • Good low-temperature properties
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.892 g/cc
Density 7.43 lb/gal
Viscosity Measurement 95Index
Kinematic Viscosity at 40°C (104°F) 227 cSt
Kinematic Viscosity at 100°C (212°F) 19.1 cSt
ASTM Color 4.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 7.6ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -28.0 °C
Flash Point 242 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 0.11 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4320 Steel, normalized at 895°C (1640°F)
AISI 4320 Steel, annealed at 850°C (1560°F)
AISI 4320 Steel, normalized 895°C (1640°F), air cooled, 13 mm (0.5 in.) round
AISI 4320 Steel, direct quench from pot (carburized 925°C (1700°F) for 8 hrs., quenched in agitated oil, 150°C (300°F) temper), 1.5 mm case depth
BASF Ultraform® H 4320 Q600 POM

WCON6308 / 210106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.