MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP)  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-processable thermoplastic. The unique properties of this material are due primarily to the rigid-rod chemical structure. PrimoSpire® SRP is differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement. In addition, it offers scratch resistance, great friction and wear properties, excellent solvent resistance and exceptional low temperature performance.

Features: Balanced Stiffness/Toughness; Ductile; Flame Retardant; Good Chemical Resistance; Low Temperature Resistant

Uses: Aircraft Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications

Additional Properties: Dynatup - ASTM D3763 58.0 J

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 115 MPaASTM D638
Elongation at Break 15 %5 mm/min; ASTM D638
Tensile Modulus 3900 MPaASTM D638
Flexural Strength 164 MPaASTM D790
Flexural Modulus 4000 MPaASTM D790
Izod Impact, Notched 69.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 171 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 370 °C
Front Barrel Temperature 375 °C
Nozzle Temperature 374 °C
Melt Temperature 375 °C
Mold Temperature 135 - 160 °C
Drying Temperature 150 °C
@Time 14400 sec
Shot Size 30 - 70 %
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormPellets
Processing TechniqueCompression Molding; Film Extrusion
 Injection Molding; Machining; Profile Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-9250 Polyphenylene, Self-Reinforced (SRP)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-9120 Self-reinforced Polyphenylene
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP)

PSOL8Y7231 / 176962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.