MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 246M PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.

Available in: Europe and North America

Product Applications: TECHNYL® A 246M offers an excellent notched impact resistance at low temperature make it suitable for: sports and leisure applications, for shoe soles, ski components, ski and surf bindings, toy applications, such as, the bumper of a remote-controlled car. This product is available in natural, white and black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183/A
Water Absorption 1.05 %
@Temperature 23.0 °C,
Time 86400 sec
1.05 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/in
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psiISO 527 Type 1A
Tensile Strength, Yield 47.0 MPa6820 psiISO 527 type 1 A
 50.0 MPa7250 psiASTM D638
Tensile Modulus 1.90 GPa276 ksiISO 527 Type 1A
Flexural Strength 70.0 MPa10200 psiISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
Izod Impact, Notched (ISO)  22.0 kJ/m²
@Temperature -30.0 °C
10.5 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1eA
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1eA
Charpy Impact Unnotched  1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 9.10 J/cm²43.3 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.23.2IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 450 V450 VSolution B; IEC 60112
 575 V575 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
Oxygen Index 24.5 %24.5 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone260-280°C
Mixing Zone270-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax TYC007P BLK Thermoplastic Olefinic Elastomer, mineral Filled
Borealis Daplen™ EF210AE Polypropylene TPO Compound
Borealis Daplen™ EF209AE Polypropylene TPO Compound
Domo Technyl® A 246M Nylon 66, Impact Grade, EH0
Borealis Daplen™ EE255AE Polypropylene TPO Compound

PRHOD699 / 137930

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.