MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group EP 2KSP EPI Engineered Polymers Silicone Modified Polyurea
Categories: Polymer; Thermoset; Polyurethane, TS; Silicone

Material Notes: EP 2KSP Polyurea, “Powered by Reactamine® Technology”, is a 2 Component polyurea that reacts with aliphatic isocyanates to produce a high gloss, chemical resistant coating EP 2KSP can be used on a variety of substrates such as bed liners, concrete, wood, metal and plastic for interior and exterior applications. EP 2KSP should be sprayed on bed liners, but can be rolled or sprayed on other surfaces at about 3-4 mils.

Key Benefits include: High gloss, Excellent chemical resistance, Quick drying, Excellent surface hardness, Excellent compatibility with polyurethane dispersions and other acrylic emulsions.

Coalescing Solvents: Butyl glycol, Butyl diglycol, Dowanol DPM, Dowanol PM, Dowanol DPnB, Dowanol TPnB, Dowanol PnB, propylene glycol butyl-acetate, Propylene glycol, NMP, Methoxybutanol, Ethanol, Lusolvan FBH, Proglide DMM.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
 8.91 lb/ft³
Solids Content 35 %
pH 7.5 - 8.5
Brookfield Viscosity 40 - 100 cPRVT, Spindle 2, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Abrasion 4.7mg loss
 
Processing PropertiesOriginal ValueComments
Processing Temperature 17.0 °CMinimum Film Formation Temperature
Cure Time <= 1.00 hour
@Thickness 0.152 mm,
Temperature 75.0 °C
Pot Life <= 60 min
 
Descriptive Properties
ColorClear
Hot TireNo Stain
Plasticizer (1 hour)50 (Failure)-5 (Excellent)
Resistance to Acetone (10 seconds)Excellent
Resistance to Alcohol (1 hour)40 (Failure)-5 (Excellent)
Resistance to Alcohol/Water 1:1 (1 hour)Excellent
Resistance to Ammonia (1 hour)Excellent
Resistance to Brake Fluid (2 hours)No effect
Resistance to Brake Fluid (24 hours)Failure
Resistance to Coffee (16 hours)Excellent
Resistance to Diesel Fuel (24 hours)No effect
Resistance to GasolineNo effect
Resistance to Motor Oil (24 hours)No effect
Resistance to Nivea (16 hours)Excellent
Resistance to Pepsi Cola (24 hours)No effect
Resistance to Transmission Fluid (24 hours)No effect
Resistance to Water (16 hours)Excellent
StabilizationAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group ReactAmine® EP 350 EPI Engineered Polymers Polyurea
CHT Group 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Covestro Bayhydrol® A 242 Polyurethane Coating
CHT Group SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea

PACC097 / 22224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.