MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea
Categories: Polymer; Thermoset; Silicone

Material Notes: EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be processed to produce elastomers of varying hardness. Water absorption of this product is shown to be five to ten times lower than regular polyureas. These elastomers were subjected to a severe hydrolysis test which involves immersing them in water at 90 °C. for a period of 28 days. A similar test has been used for military applications, where specimens are conditioned for 28 days at 100 °C and 95 % relative humidity, stimulating about 10 years of service at 35 °C. and 95 % relative humidity. The EP 82 shows excellent resistance to oxidizing agents, such as those used to treat swimming pools. Thus, chlorinated water resistance of elastomers produced from EP 82 and isocyanates, are superior to those obtained from a conventional polyurea.

Applications: electrical encapsulation, swimming pool filter end-caps, re-enterable encapsulants, cable splicing, and others where the polyurea is exposed to a hard, moisture laden environment, requiring hydrophobic resins that can provide pli necessary resistance to (i) water ingress, (ii) degradation of physical properties and (iii) corrosion of electrical components.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 11 %11 %7 days
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 606012 hours post cure.
 67
@Temperature 23.0 °C
67
@Temperature 73.4 °F
 72
@Temperature 23.0 °C
72
@Temperature 73.4 °F
Tensile Strength 14.51 MPa2104 psiAfter 28 days, 90°C H2O
 15.80 MPa2291 psiAfter 14 days, 90°C H2O
 16.12 MPa2338 psi12 hours post cure
 19.48 MPa
@Temperature 23.0 °C
2826 psi
@Temperature 73.4 °F
Elongation at Break 70 %70 %12 hours post cure
 56 %
@Temperature 23.0 °C
56 %
@Temperature 73.4 °F
Tear Strength 83.6 kN/m477 pliDie C
 115 kN/m654 pliDie C
Taber Abrasion, mg/1000 Cycles 253
@Temperature 23.0 °C
253
@Temperature 73.4 °F
 
Descriptive Properties
Resistance to Chlorinated Water Resistance+2.7 Tensile Change
 +5.6 Tear Strength ChangeTear Strength Change
 0 Hardness Change
 0% Elongation Change
 Slight DiscolorationAppearance Change

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea
CHT Group ReactAmine® EP 350 EPI Engineered Polymers Polyurea
CRG Industries Essemplex AF34 Thermoplastic Shape Memory Polymer Resin
SpinTech Veritex™ Shape Memory Polymer Composite
CRG Industries Essemplex AB43 Thermoplastic Shape Memory Polymer Resin

PACC101 / 22228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.