MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Hexene Copolymer (Barefoot)

Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.

A Hexene Copolymer Linear Low Density Polyethylene for film applications including cast stretch film and high quality packaging films requiring clarity and toughness. Available with different additive packages.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Film properties measured on 20 micron cast film extruded at 1000 ft/min with a melt temperature at 510°F. Actual film properties may vary depending on operating conditions.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 20.0 microns0.787 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 915 %915 %ASTM D882
Elmendorf Tear Strength, MD 11.6 g/micron295 g/milASTM D1922
Elmendorf Tear Strength, TD 24.7 g/micron628 g/milASTM D1922
Dart Drop 3.66 g/micron93.0 g/milASTM D1709
Film Tensile Strength at Break, MD 44.82 MPa6500 psiASTM D882
Film Tensile Strength at Break, TD 34.47 MPa5000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 1.7 %1.7 %ASTM D1003
Gloss 98 %98 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
ExxonMobil LLDPE LL 6202.19 Linear Low Density Polyethylene Resin
ExxonMobil LL 6202.19 Injection Molding Resin

PFPCPE47 / 38854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.