MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LL 6202.19 Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear resistance and low warpage.

Availability: Latin America, North America and South America

Applications:

  • Caps
  • Closures
  • Lids
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D4883
ESCR 10% Igepal® 180 hour180 hourCondition B; ASTM D1693
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 12.4 MPa1800 psiASTM D638
Elongation at Break 750 %750 %ASTM D638
Flexural Modulus 0.407 GPa
@Strain 2 %
59.0 ksi
@Strain 2 %
Secant; ASTM D790
Flexural Modulus, 1% Secant 455 MPa66000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FASTM D3418
Vicat Softening Point 96.7 °C206 °FASTM D1525
 
Descriptive Properties
FeaturesStandard processing antioxidants
FormPELLET

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil C4LL 12026.19 ExxonMobil™ Linear Low Density Polyethylene Resin
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
ExxonMobil C6LL 6836.67 Linear Low Density Polyethylene Resin
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade

PEXB211 / 37516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.