MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil C6LL 6836.67 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: ExxonMobil™ C6LL 6836.67 resin is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal warpage and outstanding toughness for cold temperature durability

Availability: Latin America and North America

Additive:

  • Thermal Stabilizer: Yes
Applications:
  • Caps and Closures
  • Cargo handling boxes
  • Large Lids
  • Large Part Housewares

Information provided by ExxonMobil

Key Words: LLDPE LL 6407.67
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ExxonMobil method
ESCR 10% Igepal® >= 1000 hour>= 1000 hourF50; ASTM D1693B
Melt Flow 6.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.9 MPa2600 psiASTM D638
Elongation at Break 760 %760 %ASTM D638
Flexural Modulus 0.565 GPa
@Strain 2 %
82.0 ksi
@Strain 2 %
Secant; ASTM D638
Flexural Modulus, 1% Secant 662 MPa96000 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 109 °C228 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LL 6407.67 Injection Molding Resin
Covestro Makrolon® 3158 Polycarbonate
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Delrin Delrin® 511DP NC010 POM

PEX99171 / 175407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.