MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: EMERGE™ PC/PET 9500CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipment housings and other applications that are subject to repeated exposure to a variety of cleaners and disinfectants commonly used in hospitals. This grade has good aesthetics and excellent toughness. It has a UL 94 rating of V-0 at 2.0 mm.

Main Characteristics:

  • Tested under ISO 10993 (Parts 5 & 10)
Applications:
  • Medical device housings or enclosures

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0095 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 in/inASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 13 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110
@Thickness 3.20 mm
Injection Molded; ASTM D785
Tensile Strength at Break 45.0 MPa
@Thickness 3.20 mm
Injection Molded, 50 mm/min; ASTM D638
Tensile Strength, Yield 53.0 MPa
@Thickness 3.20 mm
Injection Molded, 50 mm/min; ASTM D638
Elongation at Break 150 %
@Thickness 3.20 mm
Injection Molded, 50 mm/min; ASTM D638
Elongation at Yield 4.1 %
@Thickness 3.20 mm
Injection Molded, 50 mm/min; ASTM D638
Tensile Modulus 2330 MPa
@Thickness 3.20 mm
Injection Molded, 5.0 mm/min; ASTM D638
Flexural Strength 82.0 MPa
@Thickness 3.20 mm
Injection Molded, 1.3 mm/min; ASTM D790
Flexural Modulus 2270 MPaInjection Molded, 1.3 mm/min; ASTM D790
Izod Impact, Notched 750 J/m
@Thickness 3.20 mm
Injection Molded; ASTM D256
Dart Drop, Total Energy 45.0 J
@Thickness 3.20 mm,
Temperature 23.0 °C
Injection Molded, Peak Energy; ASTM D3763
 49.0 J
@Thickness 3.20 mm,
Temperature 0.000 °C
Injection Molded, Peak Energy; ASTM D3763
 60.0 J
@Thickness 3.20 mm,
Temperature 23.0 °C
Injection Molded; ASTM D3763
 62.0 J
@Thickness 3.20 mm,
Temperature 0.000 °C
Injection Molded; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmIEC 60093
Surface Resistance 5.20e+15 ohmIEC 60093
Dielectric Constant 3.12
@Frequency 1e+6 Hz
IEC 60250
 3.28
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.20 mm
in Oil; IEC 60243-1
 31.0 kV/mm
@Thickness 1.60 mm
in Oil; IEC 60243-1
Dissipation Factor 0.0030
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 74.0 µm/m-°C
@Temperature -40.0 - 80.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 109 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °CUnannealed; ASTM D648
Vicat Softening Point 140 °CASTM D1525
Flammability, UL94 V-1
@Thickness 1.50 mm
 V-0
@Thickness 2.00 mm
 5VB
@Thickness 2.50 mm
Glow Wire Flammability Index 825 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 2.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 249 - 282 °C
Mold Temperature 43.0 - 66.0 °C
Drying Temperature 121 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Mitsubishi Iupilon® MB4405U PC/Polyester
LG Chemical LUPOX TE5006FH PET+PC, Injection Molding
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
A. Schulman Diamond DIAMALOY 800 Polycarbonate/Polyester Alloy

PDWST061 / 142270

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.