MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOX TE5006FH PET+PC, Injection Molding
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Flame Retardant, GWIT, CTI

Application: IT/OA, E&E (Connector)

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inASTM D955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 265 °C
10 g/10 min
@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 59.8 MPa
@Thickness 3.20 mm
8680 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 90.2 MPa
@Thickness 3.20 mm
13100 psi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Flexural Modulus 2.16 GPa
@Thickness 3.20 mm
313 ksi
@Thickness 0.126 in
2.8mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm
@Thickness 3.20 mm
2.02 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D 257
Arc Resistance <= 60 sec<= 60 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VSolution A; UL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 250 °C482 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 6.40 mm
230 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 120 °C248 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 120 °C248 °FUL 746B
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VB
@Thickness 1.60 mm
5VB
@Thickness 0.0630 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 245 - 255 °C473 - 491 °F
Middle Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 255 - 265 °C491 - 509 °F
Nozzle Temperature 260 - 270 °C500 - 518 °F
Melt Temperature 255 - 270 °C491 - 518 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 120 °C
@Time 14400 - 21600 sec
248 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
A. Schulman Diamond DIAMALOY 800 Polycarbonate/Polyester Alloy
Covestro Makroblend® EL-700 Polycarbonate + Polyester Blend
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Mitsubishi Iupilon® MB 2112N PC/Polyester

PLHCHEM9748 / 239264

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.