MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makroblend® EL-700 Polycarbonate + Polyester Blend
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP

Material Notes: (PC+PET) blend; unreinforced; flame-retardant; impact modified; injection molding grade. Good impact strength, dimensional stability and chemical resistance. Uses include indoor electrical enclosures.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% R.H.; ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inb.o. ISO 2577
Melt Flow 19 g/10 min
@Load 5.00 kg,
Temperature 270 °C
19 g/10 min
@Load 11.0 lb,
Temperature 518 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  4100 N
@Temperature 23.0 °C
922 lb (f)
@Temperature 73.4 °F
Max force; ISO 6603-2
 5200 N
@Temperature -30.0 °C
1170 lb (f)
@Temperature -22.0 °F
Max force; ISO 6603-2
Tensile Strength at Break 57.0 MPa8270 psi50 mm/min; ISO 527-1/2
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ISO 527-1/2
Elongation at Break 100 %100 %Nominal, 50 mm/min; ISO 527-1/2
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527-1/2
Tensile Modulus 2.35 GPa341 ksi1 mm/min; ISO 527-1/2
Flexural Strength 86.0 MPa12500 psi2 mm/min; ISO 178
Flexural Yield Strength 72.0 MPa
@Strain 3.5 %
10400 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Charpy Impact, Notched  3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
Puncture Energy  45.0 J
@Temperature 23.0 °C
33.2 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 50.0 J
@Temperature -30.0 °C
36.9 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 123 °C253 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1,-2
Vicat Softening Point 136 °C
@Load 5.10 kg
277 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL Recognized
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL Recognized
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL Recognized
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FInjection Molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized
A. Schulman Diamond DIAMALOY 800 Polycarbonate/Polyester Alloy
LG Chemical LUPOX TE5006FH PET+PC, Injection Molding
ABW Polymers PC/PET Alloy
Mitsubishi Iupilon® MB 2112N PC/Polyester

PB10218 / 26256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.