MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Nevertheless, the viscosity features are on the level of PA6. Especially after storage, e.g. at 150° AKROMID RM shows comparable ageing characteristics. For appliances with very constant features, low warpage, very good finish together with an improved chemical resistance and for production of parts according to the GIT/WIT process, the version B3 GF 30 RM 9 black (3099) or respectively B3 GF 50 9 RM black (3147) offers an ideal solution. However, if a very good impact strength is predominant, our type B3 GF 30 RM black (3016) or respectively B3 GF 50 RM black (3146) will be favored.

High quality surface finish:
B3 GF 30 9 RM black (3099)/B3 GF 50 9 RM black (3147)
Very constant features with regard to climate
Very low warpage
Very good surface
CaCI2 resistant

Cost-effective:
B3 GF 30 RM black (3016)/B3 GF 50 RM black (3146)
Closer to PA 6 GF 30/GF 50
Constant features with regard to climate
Low warpage
Tendentious higher impact strength
Tendentious higher notched impact

Applications:

Electronic market:
e.g. sensor housings, coil former (wo.UL), plug-in connectors, plug panels etc.
Automobile market:
e.g. sensor housing, electrical parts, wind screen wiper bows, door handles, mirror elements, sliding roof frames etc.
General mechanical engineering:
e.g. control elements in printer, copier, housings of valves, pumps etc.

Information from Akro-Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccISO 1183
Filler Content 50 %ISO 1172
Moisture Absorption 1.2 %
@Temperature 70.0 °C
62% RH, Humidity; ISO 1110
 0.450 %
@Temperature 70.0 °C,
Time 180000 sec
62% RH
 0.700 %
@Temperature 70.0 °C,
Time 720000 sec
62% RH
 1.00 %
@Temperature 70.0 °C,
Time 1.44e+6 sec
62% RH
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4
Spiral Flow 50.0 cm7 x 4 [mm] diameter
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 280 MPaH 961/30; ISO 2039-1
Tensile Strength at Break 210 MPa5 [mm/min]; ISO 527-2/5
Tensile Strength 160 MPa
@Temperature 70.0 °C,
Time 1.44e+6 sec
62% RH
 175 MPa
@Temperature 70.0 °C,
Time 720000 sec
62% RH
 180 MPa
@Temperature 70.0 °C,
Time 180000 sec
62% RH
Elongation at Break 2.2 %5 [mm/min]; ISO 527-2/5
Tensile Modulus 16.0 GPa1 [mm/min]; ISO 527-2/1
 13.5 GPa
@Treatment Temp. 70.0 °C,
Time 1.44e+6 sec
62% RH
 14.0 GPa
@Treatment Temp. 70.0 °C,
Time 720000 sec
62% RH
 15.0 GPa
@Treatment Temp. 70.0 °C,
Time 180000 sec
62% RH
Charpy Impact Unnotched 6.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °CDIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 210 °CUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 165 °CUnannealed; ISO 75-2/C
Flammability, UL94 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 60.0 - 80.0 °C
Nozzle Temperature 240 - 280 °C
Zone 1 225 - 300 °C
Zone 2 225 - 300 °C
Zone 3 225 - 300 °C
Zone 4 225 - 300 °C
Melt Temperature 260 - 300 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 4.00 - 12.0 hour
Hold Pressure 75.0 MPa
Back Pressure 5.00 - 10.0 MPa
 
Descriptive Properties
AcetonePass100% Conc
BenzenePass100% Conc
BenzolPass100% Conc
BiodieselPass50°C, 100% Conc
Brake Fluid (DOT4)Fail130°C, 100% Conc
 Pass100% Conc
Calcium chloride, alcoholicFail10% Conc
 Pass10% Conc, when surface treated with 4 (chemical-stabilized)
Calcium chloride, aqueousFail10% Conc
 Pass10% Conc, when surface treated with 4 (chemical-stabilized)
Citric acidPass10% Conc
Diesel fuel (DIN 51601)Pass100% Conc
Sulfuric AcidFail96% Conc
ToluenePass100% Conc
WaterPass100% Conc
Zinc chloride, aqueousFail50% Conc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 50 1 natural (2531) PA 6 Conditioned, 50% Glass Filled
Envalior Akulon® K224-G0 PA6-GF50, Dry, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 50 1 natural (2531) PA 6 Dry, 50% Glass Filled
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Akro-Plastic Akromid® B3 GF 50 9 RM-M natural (3698) PA 6 Dry, 50% Glass Filled

PAKRO095 / 126875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.