MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dover Chemical CHLOREZ 700S Solid Chlorinated Alkane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chlorez 700S is a solid, 70% chlorinated alkane which is used in a variety of applications including paints, coatings, rubber, adhesives, polyolefins, textiles & fabrics. Chlorez 700S is used primarily as a flame retardant and shows excellent synergies with antimony trioxide. Additionally, ancillary improvements in various grades of rubber have been seen with improvements in both tensile and tear properties. In polyolefins, Chlorez 700S is generally recommended for use in standard grades of low-density polyethylene. In mineral filled polypropylene composites, Chlorez 700S has been used as a coupling agent.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc
@Temperature 25.0 °C
1.60 g/cc
@Temperature 77.0 °F
Bulk Density 1.619 g/cc0.05849 lb/in³
Particle Size 95 µm95 µm%, thru 297 mic
 
Thermal PropertiesMetricEnglishComments
Softening Point 103 °C217 °FASTM D36
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 - 48.0 Month
@Temperature <=37.8 °C
24.0 - 48.0 Month
@Temperature <=100 °F
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 71 %71 %
 
Descriptive Properties
Heat Stability, %0.05HCI
Physical Formwhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER009 / 217628

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.