Heat stabilized, lubricated nylon 6 intended for use in coating wire, usually extrusion coated over a layer of PVC on electrical wires for toughness, temperature resistance, and insulating properties, and contains a high slip additive for ease of use when pulling wire through conduit. Delivered dry, with less than 0.2% moisture, and can be extruded as received. Testing conducted on dry as molded specimen Information provided by Nylene® Global Polymer Solutions. |