MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ineos K44-06-122 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 3408, NSF Standard 14 certification, and compiles with ANSI/NSF Standard 61 health effects requirements. The hydrostatic design basis is 1600 psi at 23°C or 1000 psi at 60°C, based on ASTM test number D 2837. According to ASTM F 1473, the notch tensile (PENT) is greater than 100 hours. The cell classification is 345464A (ASTM D3350).

Key Words: Extrusion of potable water, industrial, and mining pipe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D4883
ESCR 100% Igepal® >= 1000 hour>= 1000 hourCondition B, F50; ASTM D1693
Oxidative Induction Time (OIT) >= 20 min
@Temperature 210 °C
>= 20 min
@Temperature 410 °F
ASTM D3895
High Load Melt Index 6.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 100 hour>= 100 hourNotch Tensile; ASTM F1473
Hardness, Shore D 6666ASTM D2240
Tensile Strength, Ultimate 27.6 MPa4000 psi2 in/min.; ASTM D638
Tensile Strength, Yield 20.7 MPa3000 psi2 in/min.; ASTM D638
Elongation at Break >= 700 %>= 700 %2 in/min.; ASTM D638
Elongation at Yield 11.2 %11.2 %2 in/min.; ASTM D638
Flexural Modulus 0.758 GPa
@Strain 2 %
110 ksi
@Strain 2 %
Secant-Method 1; ASTM D790
Izod Impact, Notched 6.00 J/cm11.2 ft-lb/inASTM D256
Hydrostatic Design Basis 6.89 MPa1000 psiat 60°C; ASTM D2837
 11.0 MPa1600 psiASTM D2837
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -118 °C<= -180 °FASTM D 746
 
Descriptive Properties
Cell Classification345464AASTM D3350
ProcessPipe Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K44-08-122 HDPE
Ineos TUB 121N HDPE
Ineos TUB 121NTW HDPE
Ineos K38-20-188 HDPE
Ineos K44-24-122 HDPE

PSOLKM006 / 68237

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.