MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Dow Dow™ 690 HEALTH+™ LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: DOW LDPE 690 HEALTH+™ is a LDPE barefoot resin designed for extrusion blow molding, injection blow molding, and blow-fill seal applications with good flexibility, moderate rigidity and good chemical resistance. It is also suitable for medical packaging films.
Main Characteristics:
  • Good flexibility
  • Good chemical resistance
  • Good stiffness

Complies with: US FDA 21 CFR 177.1520©2.2a; USP Class VI; Drug Master File Listing; Canadian HPFB No Objections; EU No 10/2011. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objections

Form: Pellets

Processing Method: Extrusion Blow Molding; Injection Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.3 MPa
@Thickness 0.0508 mm
1790 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Yield, TD 12.1 MPa
@Thickness 0.0508 mm
1760 psi
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, MD 420 %
@Thickness 0.0508 mm
420 %
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, TD 670 %
@Thickness 0.0508 mm
670 %
@Thickness 0.00200 in
ASTM D882
2% Secant Modulus  0.181 GPa
@Thickness 0.0508 mm
26.2 ksi
@Thickness 0.00200 in
MD; ASTM D882
 0.207 GPa
@Thickness 0.0508 mm
30.0 ksi
@Thickness 0.00200 in
TD; ASTM D882
Elmendorf Tear Strength MD 500 g
@Thickness 0.0508 mm
500 g
@Thickness 0.00200 in
ASTM D1922
Elmendorf Tear Strength TD 280 g
@Thickness 0.0508 mm
280 g
@Thickness 0.00200 in
ASTM D1922
Dart Drop Test 150 g
@Thickness 0.0508 mm
0.331 lb
@Thickness 0.00200 in
ASTM D1709A
Film Tensile Strength at Break, MD 24.8 MPa
@Thickness 0.0508 mm
3600 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Break, TD 23.0 MPa
@Thickness 0.0508 mm
3330 psi
@Thickness 0.00200 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C233 °F
Vicat Softening Point 98.3 °C209 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 7.6 %
@Thickness 0.0508 mm
7.6 %
@Thickness 0.00200 in
ASTM D1003
Gloss 66 %
@Thickness 0.0508 mm
66 %
@Thickness 0.00200 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 112 °C233 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance35 ft-lb/in32.0 mil
Film Toughness1920 ft-lb/in3MD, 2.0 mil, ASTM D882
 2230 ft-lb/in3TD, 2.0 mil, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF471 / 311164

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.