Product Description: DOW LDPE 690 HEALTH+™ is a LDPE barefoot resin designed for extrusion blow molding, injection blow molding, and blow-fill seal applications with good flexibility, moderate rigidity and good chemical resistance. It is also suitable for medical packaging films. Main Characteristics: - Good flexibility
- Good chemical resistance
- Good stiffness
Complies with: US FDA 21 CFR 177.1520©2.2a; USP Class VI; Drug Master File Listing; Canadian HPFB No Objections; EU No 10/2011. Consult the regulations for complete details.Availability: North America Additive: Antiblock: No; Processing Aid: No; Slip: No Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objections Form: Pellets Processing Method: Extrusion Blow Molding; Injection Blow Molding Information provided by The Dow Chemical Company |