MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Altron™ PC LSG 1000 Extruded Unfilled Polycarbonate  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: Life Science Grade Polycarbonate
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.20 %IMMERSION, 24 HRS.
Water Absorption at Saturation 0.40 %ASTM D150
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 10500 psiASTM D638
Elongation at Break 100 %ASTM D638
Tensile Modulus 320000 psiASTM D638
Compressive Strength 11500 psi
@Strain 10 %,
Temperature 22.8 °C
ASTM D695
Compressive Modulus 300000 psiASTM D695
Shear Strength 9200 psiASTM D732
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.17ASTM D150
Dielectric Strength 400 kV/inASTM D149
Dissipation Factor 0.00090ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.29 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 293 °FASTM D 3418

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
Geon® Performance Solutions Vinyl Flexible XV3758 Polyvinyl Chloride, Flexible
Overview of materials for Polycarbonate, 20% Glass Filled
Overview of materials for Polycarbonate, Extruded
Overview of materials for Polycarbonate, Molded

P1SM10B5 / 171683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.