MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel

Vanadis 4 Extra is characterized by:

  • Very good ductility
  • High abrasive-adhesive wear resistance
  • High compressive strength
  • Good dimensional stability during heat treatment and in service
  • Very good through hardening properties
  • Good temper back resistance
  • Good machinability and grindability

Applications:Uddeholm Vanadis 4 Extra is especially suitable for applications where adhesive wear and/or chipping are the dominating failure mechanisms, i.e.with soft/adherent materials such as austenitic stainless steel, mild steel, copper, aluminium, etc.as work material; with thicker work material and high strength work materials. Uddeholm Vanadis 4 Extra is however also very suitable for blanking and forming of Ultra High Strength Steel Sheet, these materials place high demands on the tool steel regarding abrasive wear resistance and ductility.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³hardened to 60 HRC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 230230Soft annealed
Modulus of Elasticity 205 GPa29800 ksi(hardened to 60 HRC)
 185 GPa
@Temperature 399 °C
26800 ksi
@Temperature 750 °F
hardened to 60 HRC
 200 GPa
@Temperature 199 °C
29000 ksi
@Temperature 390 °F
hardened to 60 HRC
Impact Test 37.0 J27.3 ft-lbHRC 65, unnotched
 47.0 J34.7 ft-lbHRC 63, unnotched
 57.0 J42.0 ft-lbHRC 61, unnotched
 67.0 J49.4 ft-lbHRC 59, unnotched
 77.0 J56.8 ft-lbHRC 57, unnotched
 97.0 J71.5 ft-lbHRC 55, unnotched
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.8 µm/m-°C
@Temperature 199 °C
6.00 µin/in-°F
@Temperature 390 °F
hardened to 60 HRC
 11.7 µm/m-°C
@Temperature 399 °C
6.50 µin/in-°F
@Temperature 750 °F
hardened to 60 HRC
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
hardened to 60 HRC
Thermal Conductivity  30.0 W/m-K
@Temperature 199 °C
208 BTU-in/hr-ft²-°F
@Temperature 390 °F
hardened to 60 HRC
 30.0 W/m-K
@Temperature 399 °C
208 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened to 60 HRC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.4 %1.4 %
Chromium, Cr 4.7 %4.7 %
Iron, Fe 85.9 %85.9 %As Balance
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 3.5 %3.5 %
Silicon, Si 0.40 %0.40 %
Vanadium, V 3.7 %3.7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
Assab Steels VANADIS 4 EXTRA Cold Work Steel
Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
AISI Type S7 Tool Steel (UNS T41907)

NBUCOR14 / 15483

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.